Open Access
Table 1
The dosage of base materials
Mortar type | Group | Design concentration of sticky rice pulp /% | For compressive strength test | For flexural strength test | ||||||
---|---|---|---|---|---|---|---|---|---|---|
Sticky rice pulp /g | Tap water /g | Cement /g |
Natural accumulated sand /g | Sticky rice pulp /g | Tap water /g | Cement /g |
Natural accumulated sand /g | |||
Common cement mortar | I | 0 | 0 | 124 | 190 | 580 | 0 | 91 | 140 | 420 |
Cement mortar with sticky rice pulp | II | 0.3 | 124 | — | 91 | — | ||||
III | 0.6 | 124 | — | 91 | — | |||||
IV | 1.0 | 124 | — | 91 | — | |||||
V | 1.5 | 124 | — | 91 | — |